Abstract
Select any words in the title or abstract, or press this and choose a sentence.
The casting defect analysis and optimization using computer aided casting simulation technique plays vital role in manufacturing of metal parts and determining various casting defects. In pressure die casting, we require a quality die to prevent unfilled phenomena, weld lines, deflection and air traps and provide two overflows for filling thin section of existing part. The gating system is very critical to a die-casting die, but designing the gating system is an iterative process that can be very time-consuming and costly. The aim of this work is, (a) to identifying the best gate location for the component taking into consideration the flow balance and to avoid differential Clamp force and pressure, (b) to optimize the model of gate location, (c) Study the causality of the defects arrive and their solutions, (d) commenting on simulation results and selecting best suitable gate design for manufacturing the final part and (e) to validate the proposed approach.
Keywords
Subjects
EngineeringAsk about this article
Answers come only from this article's title, abstract and keywords, each sentence pointing to where it comes from. Your question is sent to OpenAI to write the answer. Scholars Central does not store it.
Similar by topic
Research article · 12 Nov 2015
ANALYSIS OF DEFECTS IN MANUFACTURING OF PRESSURE DIE CASTING
Research article · Jul 2014
Mathematical Modeling and Computer Simulation of Particle Gradient Distribution in a Vertical Centrifugally Cast Functionally Gradient Composite
Short communication · 11 Feb 2015
ANALYSIS OF CENTRIFUGAL CASTING DEFECTS ON THEIR MANUFACTURING PARAMETER
Research article · 26 Dec 2014
ANALYSIS OF DEFECTS IN CENTRIFUGAL CASTING BY HYBRID METHOD
More from this journal
The newest in International Journal of Innovative Research in Science, Engineering and Technology.
Review article · 2018
Tech-Care: Personal Health Monitoring and Prediction System
Research article · 2018
Spectrum Sensing Methods for Cognitive Radio: A Survey
Review article · 2018
Utilization of Food Wastes to Prepare Film Forming Biomolecules (Retracted)
Conferences in this field
Upcoming conferences in this field.
Follow
New articles from what you follow go into your email digest, once you agree to alert emails.
- JournalInternational Journal of Innovative Research in Science, Engineering and Technology
- SubjectEngineering
- BylineArticles whose byline prints “Sandeep.v. Chavan”
- BylineArticles whose byline prints “Rajeev.K.Tavildar”