Scholars Central

Conference abstractPublished 24 Sep 2018

On the way to physically correct indentation analyses

Authors: Gerd Kaupp

Ask about this article

Abstract

Select any words in the title or abstract, or press this and choose a sentence.

Common indentation analyses (ISO and ASTM standardized) suffer from iterations, polynomials and approximations. However, correct physics on the basis of elementary mathematics avoids iterations and violations of the energy law for hardness and modulus. The new physically founded laws FN=0.8 k h3/2 and Wapplied/Windent =5/4 apply to nano, micro and macro depth sensing indentations. Importantly, they detect phase changes under load and allow for the arithmetic treatment for single or successive phase transformations, surface layer effects and correct adsorption energies. Thus, the first physical hardness H, stiffness/indentation moduli (these are not "Young's moduli"), indentation works, activation energies and phase transformation energies are directly obtained, simply by application of the basic physically founded equations that avoid the unfortunate common energy law violations. Non-steadiness kinks (in the linear h3/2 plots) and any deviations from the precise 5/4 ratio (integration of the smooth appearing loading curves over one or more phase transition onsets is not allowed) prove phase change (s) under load. For example, five successive phase changes to reveal six different polymorphs of NaCl up to 50 N load (corresponding to HV5) from depth-sensing indentations will be presented and analysed. In addition to fcc and bcc, theoretical predictions published three new polymorph structures and there is the possibility of twins and amorphous phases. The undeniable half-page physical deductions of the two basic formulas will be presented and discussed as the derived formulas for the mentioned and further mechanical applications. This is not only of academic interest, but materials' properties must be correctly and reliably described, and technical materials must withstand pressure upon use without failing. The latter are at risk when phase change onset pressures remain undetected, because of the formed interfaces between different polymorphs as sites for nucleation of cracks. Highly resolved (5000X) 3D-microscopy reveals details of crack nucleation. The non-detection of of phase changes is the main objection against the reliability of non-depth-sensing Vickers, Brinell, Rockwell, etc. hardness characterizations of daily life technical materials (not withstanding their always similar standard plates that equally undergo the undetected phase changes). The neglecting of always several undetected phase changes misses the most relevant properties with creation of high common risks. Furthermore, indentation measurements gain enormously in precision, because invalid single measurements can be directly excluded when they do not concur with the undeniable physical FN h3/2 law's linear correlation with >3 or >4 nines, due to local imperfections, or skew, or too close to interface or to borderline indentations. The safety issues also for all the numerous applications that derive from ISO H and Er are evident and largely unexplored.

Ask about this article

Answers come only from this article's title, abstract and keywords, each sentence pointing to where it comes from. Your question is sent to OpenAI to write the answer. Scholars Central does not store it.

Try:

Similar by topic

More from this journal

The newest in Research & Reviews: Journal of Material Sciences.

All its articles

Conferences in this field

Upcoming conferences in this field.

Follow

New articles from what you follow go into your email digest, once you agree to alert emails.

  • JournalResearch & Reviews: Journal of Material Sciences
  • SubjectMaterials Science
  • BylineArticles whose byline prints “Gerd Kaupp”

For authors and organisers

Publish, present and keep up with your field

Find the right journal for your paper and submit your manuscript.

Photo: Pexels