Conference abstractPublished 20 Mar 2017
Fabrication of low resistive and stable Li-P co-doped p-type ZnO by dual ion beam sputtering
Indian Institute of Technology Indore, India
Abstract
Select any words in the title or abstract, or press this and choose a sentence.
In the last decade, Zinc oxide (ZnO) based optoelectronic devices have attracted much attention due to their superior material properties such as wide direct band gap energy, large exciton binding energy, high radiation resistance and chemical and thermal stability. However, the lack of availability of reliable and stable p-type ZnO has always remained a concern in order to fabricate these devices. Various groups have reported p-type ZnO by doping with different elements of group V, whereas others have also used co-doping approach for achieving p-type conduction in ZnO. Unfortunately, the high resistivity and low hole concentration still poses limitations for high performance devices. In this work, we report the fabrication of high hole concentration, low resistive and stable Li-P co-doped ZnO (LPZO) thin films. LPZO thin films were fabricated by DIBS technique on low resistive n-type Si substrates. The deposition was performed using high quality ceramic target having Li and P content of 5% and 3% respectively, in oxygen rich ambient at 300 oC and 500 oC. Post deposition annealing was carried out in N2 ambient at 800 oC for 20 minutes to activate the acceptor dopants. The XRD pattern of annealed LPZO film confirmed that crystal structure was preferentially oriented in c-axis (002) direction. FWHM of (002) peak was calculated to be 0.24o resulting in a crystallite size of ~35 nm. Figure 1(a) shows the schematic structure of p-LPZO/n-Si heterojunction with linear I-V curves of ohmic contacts. Hall measurement was performed in the van der Pauw configuration to measure the electrical parameters e.g., carrier concentration, resistivity and mobility. The annealed LPZO films clearly depicted p-type conduction as observed from the rectifying behavior shown in Figure 1(b). A relatively higher hole concentration of the order 2×1020 cm-3 and resistivity of 8×10-3 Ω.cm were calculated. The turn-on voltage of the diode was determined to be 1.6 V whereas the rectification ratio of forward to reverse current at ±3 V was 76.
Ask about this article
Answers come only from this article's title, abstract and keywords, each sentence pointing to where it comes from. Your question is sent to OpenAI to write the answer. Scholars Central does not store it.
Follow
New articles from what you follow go into your email digest, once you agree to alert emails.
- BylineArticles whose byline prints “Pankaj Sharma”