Select any words in the title or abstract, or press this and choose a sentence.

Ceramic shaping processes such as uniaxial pressing, tape casting or extrusion favor the orientation of clay platelets in silicate materials. For example, kaolinite and muscovite phyllosilicates exhibit an anisotropic structure having attracted considerable interest in optimizing materials characteristics. As a consequence, mechanical and thermal properties can be significantly different in function of considered directions. However, controlling thermal treatment is also essential in such materials to keep the anisotropic microstructure of specimens after sintering and to optimize amount, organization and size of the occurred mullite phase. Moreover, adding a slight proportion of a second phase such as low cost silicate-based long fibres can also contribute to enhance mechanical properties. In this work, two types of silicate ceramic materials are presented: Clay-based materials obtained by extrusion processing anisotropy at macroscopic scale has been evidenced by thermal conductivity (laser flash method) and YoungâÂ?Â?s modulus (pulse echography technique) measurements denoting a decrease of anisotropic degree when the temperature of sintering increases. These results are in agreement with significant transformations occurring in kaolinite phase; multi-layer ceramic composites reinforced with silicate-based fibres, it has been shown that mechanical properties of final substrate specimens are closely related to the organization degree of mullite crystals, due to the formation of a specific mullite network at different scales of the microstructure. The anisotropy of elastic properties has also been evidenced in directions parallel and perpendicular to the casting direction. Despite the very low proportion of added fibres (less than 5 wt.%), YoungâÂ?Â?s modulus and stress to rupture are improved to about 20 and 50% respectively. Moreover, fracture toughness values are multiplied at least by 2 compared to the single substrate layer because of crack defection and crack bridging mechanisms occurring at the fiber/matrix interface.

Ask about this article

Answers come only from this article's title, abstract and keywords, each sentence pointing to where it comes from. Your question is sent to OpenAI to write the answer. Scholars Central does not store it.

Try:

More from this journal

The newest in Journal of Material Sciences & Engineering.

All its articles

Conferences in this field

Upcoming conferences in this field.

Follow

New articles from what you follow go into your email digest, once you agree to alert emails.

  • JournalJournal of Material Sciences & Engineering
  • SubjectEngineering
  • SubjectMaterials Science
  • BylineArticles whose byline prints “Nicolas Tessier-Doyen”

For authors and organisers

Publish, present and keep up with your field

Find the right journal for your paper and submit your manuscript.

Photo: Pexels