oxidant on the conductivity of Polythiophene and Polyvinyl acetate composite films. The X-ray diffraction technique is used for the determination of amorphous nature. The temperature dependence of conductivity showed
thin films on different substrates by Chemical Bath Deposition Method. We record X-ray diffraction pattern and SEM of the developed samples. It is found that, the average grain size
rather than crystallite size and hence has been studied with respect to X-ray diffraction (XRD) and Transmission Electron Microscopic (TEM) images followed by UV-VIS study to obtain
complexing agent. The nanoparticles were characterized using techniques such as X-ray powder diffraction (XRD), scanning electron microscope. (SEM), UV–VIS absorption spectroscopy, and photoluminescence spectroscopy…
either in single step or decompose through respective metal carboxylate intermediates. X-ray powder diffraction patterns of the complexes are almost superimposable with in each of the series indicating isomorphism
Formation of cobaltite has been confirmed by thermogravimetry (TG) weight loss and X-ray diffraction. Combustion of the precursor in air yields fine powder of cobaltites with large surface area
this article. Scanning electron microscope (SEM), X-ray photoelectron spectroscopy (XPS), X-ray diffraction (XRD) was used to study the impact of surface composition and surface microstructure
capping agent. The NP preparations were characterized using UV–VIS absorption spectroscopy, X-ray diffraction (XRD), Fourier Transform infrared spectroscopy (FTIR) and scanning electron microscopy (SEM) analyses
TOPO) as the capping agent at 120ºC for 2 hrs. Electron microscopy, X-ray diffraction, and absorption spectra have been used to investigate the products, and the mechanism is proposed
first time.The commercial sample was characterized by Fourier-transform Infra-red FTIR) spectroscopy, Xray diffraction XRD) analysis, scanning electronmicroscopy SEM) as well as by atomic absorption spectroscopy AAS)…
thermal treatment. The structure of the sample prepared was studied using X-ray Diffraction (XRD), Energy dispersive X-Ray Spectroscopy (EDS), High Resolution Transmission ElectronMicroscopy
contained glycerol. The clay dispersion in the films was analyzed by XRD (X-ray diffraction). XRD test showed that the clay nanolayers formed an exfoliated structure. The effect ofMMT loading
Structural and optical properties were investigated by using energy dispersive spectroscopy (EDS),X-Ray diffraction (XRD), Scanning electronmicroscope (SEM) and optical reflection and transmission measurements. The…
atmosphere at 750°C for 90 min. Rutherford Backscattering Spectrometry (RBS) and X-ray diffraction (XRD) pole figure have been used to investigate the growth and the structure
ZnCdO nanocomposites have been synthesized by solvothermal process. X-ray diffraction spectra confirm that the sample is of hexagonal wurtzite structure, and a little Cd doping would not change
relative configuration of 11á-hydroxy-â-amyrin was determined by single-crystal X-ray diffraction analysis. It crystallizes in orthorhombic system, space group P212121
ethanedioate precursor at 400 °C. The nanoparticles were characterized by powderX-ray diffraction (XRD), FT-IR spectroscopy, scanning electron microscopy (SEM), transmission electron microscopy (TEM), colorimetric…
technique. The nano size structure of TiO2 was confirmed by X-Ray Diffraction Spectroscopy (XRD), Field Emission Scanning ElectronMicroscopy (FESEM). The gas sensitivity of material tested by preparing thick film
clay before and after modification were determined and compared using X-ray diffraction (XRD), Fourier transforminfra red (FTIR) and thermogravimetric analyzer (TGA). The chemical composition of bentonite was determined
composition have been determined via high resolution transmission electron microscope (TEM) and X-ray diffraction (XRD) analysis. These nanomaterials have been used as a photocalalysts for photodegradation of organic…
hexagonal structure and a strongly preferred orientation along the c-axis. X-ray diffraction analyses showed that the crystallinity of BZO films were deteriorated by addition of boron as compared
optical band gap. Structural characterization was performed using scanning electron microscopy andX-ray diffraction. Elevating the substrate temperatures from 50oC to 300oC, increased the thickness of ITOfilmsmore than…
under inert atmosphere. The obtained ingots weremetallographically prepared then characterized by electronmicroscopy, X-ray diffraction and surface fractions measurements. The calculations and metallographic results…