Fabrication and characterisation of high-frequency ultrasonic transducers based on piezoelectric thick films and porous backing
water at pH 8 followed by sintering the powder compacts at 1080 oC. Ceramic exhibited homogeneous microstructure with 15 % porosity and spherical, ~1 and ~10 Ã?µm-sized pores, respectively ... coupling coefficient of 45…