Article · 22 Jan 2026
Conference abstractPublished 16 Apr 2022
Evaluation of surface analysis of Gutta Percha after disinfecting with sodium hypochlorite, silver nanoparticles and chitosan nanoparticles by atomic force microscopy: An in vitro study
Abstract
Select any words in the title or abstract, or press this and choose a sentence.
Aims & objectives: The purpose of this study is to evaluate the surface topography of gutta percha (GP) after disinfecting with Sodium hypochlorite (5.25%), Silver nanoparticles (70 μg/ml) and chitosan nanoparticles (1.5 mg/ml) by atomic force microscopy (AFM). Materials and methods: Forty (40) Gutta percha cones were taken in this in vitro study. These samples were divided into four different groups such as: Group I – control group (untreated GP Points), Group II, III, and IV were treated with 5.25% Sodium hypochlorite (NaOCl), 70 μg/ml silver nanoparticles (AgNPs) and 1.5 mg/ml Chitosan nanoparticles (ChNPs) respectively. The surface topography analysis of the samples was performed using AFM. Statistical analysis: Root mean square (RMS) and surface roughness parameters were used to compare the structure of GP points with contact mode imaging. These values were tested by IBM SPSS-20.0 version statistical software using one-way ANOVA and Post-hoc (Tukey HSD) tests. They were considered statistically significant when P < 0.05. Results: The Root mean square (RMS) and surface roughness values are significantly higher for Sodium hypochlorite group (5.25% NaOCl) when compared with silver nanoparticles group (70 μg/ml AgNPs) and Chitosan nanoparticles group (1.5 mg/ ml ChNPs). Conclusion: This study has shown more surface topography deterioration of GP treated with NaOCl and lesser deterioration with AgNPs and ChNPs which affects postoperative prognosis.
Keywords
Subjects
Dentistry & Oral HealthAsk about this article
Answers come only from this article's title, abstract and keywords, each sentence pointing to where it comes from. Your question is sent to OpenAI to write the answer. Scholars Central does not store it.
More from this journal
The newest in Dentistry: Case Report.
Follow
New articles from what you follow go into your email digest, once you agree to alert emails.
- JournalDentistry: Case Report
- SubjectDentistry & Oral Health
- BylineArticles whose byline prints “Chavva Lakshmi Charan Reddy”