Repair of aged composite with composite: Effect of different surface treatment (In vitro study)
Abstract
Select any words in the title or abstract, or press this and choose a sentence.
Background and aim: Repair of composite restorations is a minimally invasive approach and it can reduce cost and time of dental treatment. This study aims to compare the effect of different surface treatments (phosphoric acid, hydrofluoric acid, silane with universal adhesive) on the Shear Bond Strength (SBS) of aged repaired composites. Materials and methods: Seventy cubic composite blocks (5 mm x 6 mm) were fabricated at teflon matrix made for this study, then aged by keeping in distilled water at 37C for 24 hours then at 55C for 4 days. Specimens were roughened by diamond bur and divided into 7 groups (n=10) according to surface treatment:(phosphoric acid 37% + silane + universal adhesive, phosphoric acid 37% + universal adhesive, universal adhesive, hydrofluoric acid 9.8% + silane + universal adhesive, hydrofluoric acid 9.8% + universal adhesive, universal adhesive, one block composite no therminal treatment for the first time (positive control), no surface treatment (control)). The conditioned surfaces of all specimens were covered with repair composite Cylinders (4mm x 6mm) and aged as previously. The shear bond strengths were measured for all specimens using a universal test machine (test 114). Data were collected and statistically analyzed by SPSS version 13 and using One way ANOVA Test. P-value of 0.05 was taken as statistically significant level. Results: The specimens repaired with phosphoric acid 37% + silane + universal adhesive showed the highest SBS value and were significant. There were no significant differences in SBS between phosphoric acid 37% + silane + universal adhesive and universal adhesive and positive control groups (p > 0.05). There was no significant difference at SBS values between negative control and hydrofluoric acid 9.8% + silane + universal adhesive, hydrofluoric acid 9.8% + universal adhesive groups with the lowest SBS value. Conclusion: For aged composite repair silane application after phosphoric acid etching and then adhesive application could enhance bonding between old and new composite restoration. Application of hydrofluoric acid for old composite restorations is not recommended.
Keywords
Subjects
Dentistry & Oral HealthAsk about this article
Answers come only from this article's title, abstract and keywords, each sentence pointing to where it comes from. Your question is sent to OpenAI to write the answer. Scholars Central does not store it.
More from this journal
The newest in Dentistry: Case Report.
Conferences in this field
Upcoming conferences in this field.
Follow
New articles from what you follow go into your email digest, once you agree to alert emails.
- JournalDentistry: Case Report
- SubjectDentistry & Oral Health
- BylineArticles whose byline prints “Thuraya Lazkani”