Poly (ethylene oxide) (PEO), a water soluble linear polymer, is supplied in various molecular weights ranging 100,000 to 10,000,000 Daltons. Pharmaceutical applications of PEO include being used as an agent to enhance viscosity, binding, film forming, osmotic, and controlled release properties. PEO can be processed along with active and other excipients utilizing conventional dry compaction, wet granulation, and hot melt extrusion technologies. The latter being a preferred method of formulating PEO based abuse-deterrent pain medications. The main objective of this study was therefore to determine the influence of molecular weight on the thermal properties and degradation of PEO. The commercial grades of PEO selected for this study were Polyox™ WSR 205, 1105, N12k, N60k, 301, coagulant, and 303 having respective average molecular weights of 600K, 900K, 1M, 2M, 4M, 5M and 7M. Measurement of melting point, heat of fusion, and degradation was investigated by differential scanning calorimetry (DSC) in combination with thermo gravimetric analysis (TGA). Results were obtained in the temperature range of 25-445oC for DSC (Perkin Elmer DSC 4000) and 30-500oC for TGA (PerkinElmer TGA 4000) at a rate of 10oC/min while under a nitrogen blanket (20 mL/min). The melting points of Polyox WSR 205, 1105, N12k, N60k, 301, coagulant and 303 grades were found at approximately 76.87, 77.42, 76.6, 79.34, 77.19, 77.79 and 79.22oC respectively. Heat of fusion was calculated to be approximately 136.75, 160.37, 150.02, 152.49, 153.75, 163, 154.06 J/g, respectively. Thermal degradation was observed around 400oC and was confirmed with thermo gravimetric analysis. Inflection point of all grades was 421.76, 415.29, 416.28, 415.6, 416.1, 414.43 and 416.69oC, respectively. In general, DSC measurements show no differences in thermal properties of the tested PEOs with change in molecular weight.

Ask about this article

Answers come only from this article's title, abstract and keywords, each sentence pointing to where it comes from. Your question is sent to OpenAI to write the answer. Scholars Central does not store it.

Try:

More from this journal

The newest in Analgesia & Resuscitation : Current Research.

All its articles

Conferences in this field

Upcoming conferences in this field.

Follow

New articles from what you follow go into your email digest, once you agree to alert emails.

  • JournalAnalgesia & Resuscitation : Current Research
  • SubjectAnaesthesia & Pain
  • BylineArticles whose byline prints “Srinath Muppalaneni”
  • BylineArticles whose byline prints “David Mastropietro”
  • BylineArticles whose byline prints “Hossein Omidian”