Conference abstract · 17 Dec 2025
Conference abstractPublished 27 Jul 2017
Decay in mechanical properties of sulfonated poly (ether-ether-ketone) membrane in an ex situ hygrothermal cycling test
Iran University of Science and Technology, Iran
Abstract
Select any words in the title or abstract, or press this and choose a sentence.
Statement of the Problem: One of the key challenges facing the commercialization of fuel cell technology is the durability of proton exchange membranes (PEM) especially in automotive application. Even though PEMs suffer from chemical degradation in real fuel cell condition, Mechanical degradation shouldn’t be overlooked. PEMs are exposed to humidity fluctuation and tend to swell in high humidity or shrink in low humidity. It is shown in the figure 1 that repetition of these tensile and compression forces leads to fatigue failure. Additionally, temperature affects mechanical behavior of polymeric membranes for sure, thus, accelerated hygrothermal cycles would end up to membrane failure because of the reactant cross-over through the membrane or crack formation at the end. Methodology & Theoretical Orientation: In this work, sulfonated poly(ether-ether-ketone) (sPEEK) membrane as an alternative to state of the art PFSA membranes was used due to low manufacturing cost, high operating temperature and fairly good electrochemical performance. Membranes were prepared, treated and characterized, i.e. sulfonation degree of 64.75% was calculated from H-NMR spectroscopy and ion exchange capacity and cross-linking ratio were calculated respectively. Then, hygrothermal cycles were implemented by home-made setup contains single cell with serpentine flow channels to simulate membrane’s constraint at the in situ condition. Findings: As it was shown in figure 2, membranes have a slight increment in their elastic modulus and act more brittle when exposed to these cycles and as a result, chance of crack formation or propagation increases. On the other hand, water uptake of membranes has increased dramatically up to 184%. Conclusion & Significance: PEMs in harsh fuel cell condition; according to figure 3 are in a vicious circle which can lead to its failure. Humidity fluctuation triggers the circle, and degradation continues with the increment of young module and stress every cycle. Also, the more the membrane swells, the more stress amplitude we would expect.
Subjects
Energy & PowerAsk about this article
Answers come only from this article's title, abstract and keywords, each sentence pointing to where it comes from. Your question is sent to OpenAI to write the answer. Scholars Central does not store it.
More from this journal
The newest in Journal of Fundamentals of Renewable Energy and Applications.
Conference abstract · 17 Dec 2025
Multi-energy infrastructure for production and storage of green hydrogen
Conference abstract · 17 Dec 2025
Deforestation: the last battle against human existence
Conferences in this field
Upcoming conferences in this field.
Follow
New articles from what you follow go into your email digest, once you agree to alert emails.
- JournalJournal of Fundamentals of Renewable Energy and Applications
- SubjectEnergy & Power
- BylineArticles whose byline prints “Aida Karimi”
- BylineArticles whose byline prints “Seyed Hesam Mirfarsi”
- BylineArticles whose byline prints “Milad Shakouri Kalfati”
- BylineArticles whose byline prints “Soosan Rowshanzamir”