Scholars Central

Conference abstractPublished 21 May 2018

Centrifugally spun alumina zirconia fibers

Authors: N. Thamarai Selvi, Parag Bhargava

Ask about this article

Abstract

Select any words in the title or abstract, or press this and choose a sentence.

Statement of the Problem: Ceramic fibers (micron or nano meter dia.) are being used in place of conventional refractory bricks due to their exceptional thermal insulation properties like low thermal mass, low thermal conductivity etc. There are high and low temperature methods to synthesize fibers. But the low temperature methods conserve lot of energy. Hence, sol-gel with centrifugal spinning was chosen to synthesize fibers. The purpose of this study is to synthesize alumina zirconia (stabilized and unstabilized) fibers and to understand the grain growth controlling mechanisms. Methodology & Theoretical Orientation: In the present work, alumina zirconia (5-20 wt. % zirconia) fibers were synthesized by sol-gel with centrifugal spinning. Monolithic alumina fibers had an average grain size of ~4 Ã?µm which is huge and it will degrade mechanical properties. Hence zirconia was added to control the grain growth. Findings: The diameter of the fibers was between 5-15Ã?µm. Fiber index after sieving at 90 Ã?µm sieve was around 96 %. SEM images confirmed that the fibers were devoid of any abnormal grains (Fig. 1 (a-d)). Average alumina grain size was ~ 4 Ã?µm. Alumina fibers with zirconia showed homogeneous distribution of zirconia throughout the fibers (Fig. 1 (b-d)). It was also confirmed that zirconia controlled the growth by triple junction pinning effect which is in good agreement with the mechanisms reported. With the increase of zirconia content from 5 wt. % to 20 wt. % more number of grain boundary junctions are pinned which controls the grain boundary mobility effectively. Conclusion & Significance: Alumina zirconia fibers of 5-15 Ã?µm dia. were synthesized using sol-gel with centrifugal spinning. Average alumina grain size was ~ 4 Ã?µm. This got reduced to 2.8 Ã?µm and 1.1 Ã?µm respectively for 5 and 20 wt. % and it varied in between for 10 and 15 wt. % zirconia Zirconia controlled the growth by secondary phase pinning which is in good agreement with the mechanisms reported.

Ask about this article

Answers come only from this article's title, abstract and keywords, each sentence pointing to where it comes from. Your question is sent to OpenAI to write the answer. Scholars Central does not store it.

Try:

Follow

New articles from what you follow go into your email digest, once you agree to alert emails.

  • JournalResearch & Reviews: Journal of Material Sciences
  • SubjectMaterials Science
  • BylineArticles whose byline prints “N. Thamarai Selvi”
  • BylineArticles whose byline prints “Parag Bhargava”