Thermal analyses of NaNO3-RbNO3 pseudo-binary system-differential scanning calorimetry
Abstract
Select any words in the title or abstract, or press this and choose a sentence.
The differential scanning calorimetry (DSC) in NaxRb1-xNO3 pseudo-binary systemare presented by varying x from0 to 1. The formation of an intermediate compound and its effect on the phase transitions of RbNO3 is explained in terms of redistribution of energies involved in various transitions. Corresponding phase diagramis constructed. DSC peak at about 173 C with eutectic composition 0.46 (Na mole fraction) has been attributed to the formation of a congruently melting compound NaRb(NO3)2. X-Ray Diffracto grams (XRD) indicate the formation of this newcompound. DSCpeak corresponding to the melting of this compound and XRD lines related to this compound are found to grow with x until it reaches the eutectic composition.
Subjects
Materials ScienceAsk about this article
Answers come only from this article's title, abstract and keywords, each sentence pointing to where it comes from. Your question is sent to OpenAI to write the answer. Scholars Central does not store it.
More from this journal
The newest in Materials Science: An Indian Journal.
Short communication · 31 Mar 2025
High-Performance Metallic Alloys: From Structural Applications to Functional Devices
Short communication · 31 Mar 2025
Spintronics and Magnetic Materials: Bridging Quantum Phenomena with Device Engineering
Conferences in this field
Upcoming conferences in this field.
Follow
New articles from what you follow go into your email digest, once you agree to alert emails.
- JournalMaterials Science: An Indian Journal
- SubjectMaterials Science
- BylineArticles whose byline prints “A.Sadananda chary”
- BylineArticles whose byline prints “M.V.Madhava Rao”
- BylineArticles whose byline prints “S.Narender Reddy”