Polycrystalline samples of NaxCo2O4 were synthesized by conversional solidstate reaction (SSR) method, various temperatures sintered at of 1173- 1293 K. The mechanical properties of the samples showed the crystal structure, elastic moduli and Debye temperature. The thermoelectric properties of the samples obtained the electrical resistivity, Seebeck coefficient and thermal conductivity are increases with increased sintering temperature. The dimensionless figure of merit was decreased with an increase in sintering temperature, and the sample sintered at 1173 K was a maximum values, ZT ∼ 0.11 at 973 K.

Ask about this article

Answers come only from this article's title, abstract and keywords, each sentence pointing to where it comes from. Your question is sent to OpenAI to write the answer. Scholars Central does not store it.

Try:

More from this journal

The newest in Materials Science: An Indian Journal.

All its articles

Conferences in this field

Upcoming conferences in this field.

Follow

New articles from what you follow go into your email digest, once you agree to alert emails.

  • JournalMaterials Science: An Indian Journal
  • SubjectMaterials Science
  • BylineArticles whose byline prints “Tosawat Seetawan”
  • BylineArticles whose byline prints “Ken Kurosaki”