Scholars Central

Conference abstractPublished 14 Apr 2014

Ceramic coating prevents corrosion of cardiovascular stainless steel stents

Authors: Víctor Moles, Lucila Navarro, Julio Luna, David Vetcher, Ignacio Rintoul

Ask about this article

Abstract

Select any words in the title or abstract, or press this and choose a sentence.

Ninety percent of coronary percutaneous interventions (PCI) consist in stenting to restore blood flow. Arterial re- obstruction due to restenosis and thrombosis represent a limitation of PCI. These physiological responses are mainly attributed to the release of corrosion products from the metallic stents direct to endothelial tissue and blood flow. This work presents the corrosion phenomena observed in commercially available stents and the relations with its metallurgical condition, composition of the physiological environment in which they are implanted and manufacturing processes. It also includes a comparison with ceramic coated stents. Commercially available stents made of 316L steel were used. EDX, AES, SEM and metallographic techniques were used for chemical analysis, surface composition, topography and determination of metallurgical states, respectively. Stents were immersed in PBS saline solution at 37°C for 8 weeks. Periodically, the stents were withdrawn from the physiological environment to monitor the progress of corrosion. After 2 weeks of incubation, stents showed a dendritic corrosion pattern. This is associated with chemical segregation of alloying elements in the metal matrix for the effect of temperature at which the stent are subjected during its laser manufacture. At 4 weeks, the surface showed a pattern of vermicular corrosion located at the curved sections of the stent. This is related to the presence of residual stresses in the curved sectors as a result of stent crimping process made after the laser draft. After 6 weeks, stents exhibited large pits due high chloride content on the physiological medium. In the ceramic coated stents corrosion was practically zero until 6 weeks of incubation. Ceramic coating after surface passivation could be a way to reduce endothelial proliferation and restenosis.

Subjects

Cardiology

Ask about this article

Answers come only from this article's title, abstract and keywords, each sentence pointing to where it comes from. Your question is sent to OpenAI to write the answer. Scholars Central does not store it.

Try:

More from this journal

The newest in Clinical and Experimental Cardiology.

All its articles

Conferences in this field

Upcoming conferences in this field.

Follow

New articles from what you follow go into your email digest, once you agree to alert emails.

  • JournalClinical and Experimental Cardiology
  • SubjectCardiology
  • BylineArticles whose byline prints “Víctor Moles”
  • BylineArticles whose byline prints “Lucila Navarro”
  • BylineArticles whose byline prints “Julio Luna”
  • BylineArticles whose byline prints “David Vetcher”
  • BylineArticles whose byline prints “Ignacio Rintoul”