Experimental Study on Factors Affecting the Recovery of Nickel from Spent Catalyst
Abstract
Select any words in the title or abstract, or press this and choose a sentence.
In this study, the recovery of nickel from spent NiMo/Al2O3 catalyst was investigated using 1 L stainless steel autoclave batch reactor. The effect of leaching process parameters such as temperature (40-80°C), time (1-4 h), pressure (1-3 bar), average particle size (69-550 μm) and agitation speed (400-600 min-1) on nickel extraction. The nickel percent in spent catalyst was found about 2.18%. The results obtained show that recovery of about 94% of nickel from spent catalyst was accomplished under the following conditions: temperature 80°C, pressure 1 bar, average particle size 200 μm, agitation speed 600 min-1, nitric acid concentration 40% and solid to liquid ratio1:50 after 4 h.
Subjects
Materials ScienceAsk about this article
Answers come only from this article's title, abstract and keywords, each sentence pointing to where it comes from. Your question is sent to OpenAI to write the answer. Scholars Central does not store it.
More from this journal
The newest in Journal of Powder Metallurgy & Mining.
Short communication · 1 Dec 2025
Advanced ODS Alloys: Processing, Performance, and Applications
Short communication · 1 Dec 2025
Powder Compaction: Material, Process, And Application Insights
Conferences in this field
Upcoming conferences in this field.
Follow
New articles from what you follow go into your email digest, once you agree to alert emails.
- JournalJournal of Powder Metallurgy & Mining
- SubjectMaterials Science
- BylineArticles whose byline prints “Khalid MM”
- BylineArticles whose byline prints “Athraa BA”