Multiscale modeling of the atomic layer deposition of HfO2 thin film grown on silicon: How to deal with a kinetic monte carlo approach
Abstract
Select any words in the title or abstract, or press this and choose a sentence.
In this presentation we discuss briefly the principles of the multiscale modeling and its applications in nanomaterials and nanoscience through selected applications. Indeed, to investigate the atomic layer deposition (ALD) of HfO 2 on Si(100) surface, an original integrated approach developed within a multiscale strategy, which combines first-principles quantum simulations and kinetic Monte Carlo (KMC), is presented. Density functional theory within the hybrid functional is used to determine the detailed physicochemical mechanisms and associated energetics of the two half cycles taking place during the initial stage of film growth. A kinetic Monte Carlo model is then proposed that deals with the stochastic nature of the calculated DFT mechanisms and barriers. Beyond the chemical information emanating from DFT calculations, the lattice-based KMC approach requires preliminary physical considerations issued from the crystal structures that the system is intended to adopt. This is especially critical in the case of heterogeneous systems like oxides deposited on silicon. We also describe (i) how atomistic configuration changes are performed as a result of local events consisting in elementary reaction mechanisms occurring on specific lattice sites, (ii) the temporal dynamics, governed by transition probabilities, calculated for every event from DFT activation barriers, and (iii) the relation of KMC with the ALD experimental procedure. Some preliminary validation results of the whole multiscale strategy are given for illustration and pertinence with regard of the technological main issues.
Keywords
Subjects
NanotechnologyAsk about this article
Answers come only from this article's title, abstract and keywords, each sentence pointing to where it comes from. Your question is sent to OpenAI to write the answer. Scholars Central does not store it.
More from this journal
The newest in Journal of Nanomedicine & Nanotechnology.
Article · 21 Oct 2025
Green Synthesis of Chromium(III) Oxide Nanoparticles and their Evaluation against Skin Infections
Article · 19 Jun 2025
Potential of Bhasma as Nanomedicine for Disease Management: A Synopsis
Conferences in this field
Upcoming conferences in this field.
Follow
New articles from what you follow go into your email digest, once you agree to alert emails.
- JournalJournal of Nanomedicine & Nanotechnology
- SubjectNanotechnology
- BylineArticles whose byline prints “Ahmed Dkhissi”