Abstract

Select any words in the title or abstract, or press this and choose a sentence.

Fe81Ga19 alloy is an auxetic material, which means that its Poisson?s ratio along the [110] direction, V [110] , is negative. When this alloy is deposited on a single-crystal Si(100) wafer, the film is highly (110) textured. Thus, if we indent the film plane with a Berkovich indenter vertically, the apparent hardness obtained with the parameter V ef f = V [110] =-0.55 < 0 should be larger than that with V eff = V [110] =+0.30. This is reasonable, because if V eff is negative, the deformed material under the pressing indenter tends to push the tip slightly upward (or backward). As a result, the measured depth of circle of contact, hp, of this auxetic film is smaller than it should be under a fixed force, F, and, moreover, since the hardness H ≡ F/[24.5(hp)2], the apparent (measured) hardness must be larger. We have made a series of (Fe100-xCox) 81 Ga 19 /Si(100) films, and measured their hardness. The results indicate that: [1] when 0≤x<7 at %Co, the films (or alloys) are auxetic ( V eff <0); [2] when 7≤x≤11 at %Co, they are critical (V eff =0); and [3] when 11 0). Each point on the loading or un-loading curve was analyzed by the finite element analysis to show the side-view of the shear-stress (τ) distributions in the film, film/substrate, and substrate regions, respectively. We can study (or outline) the plastic-flow zone beneath the indenter by adopting the Tresca criterion: τ ≥ H/6

Ask about this article

Answers come only from this article's title, abstract and keywords, each sentence pointing to where it comes from. Your question is sent to OpenAI to write the answer. Scholars Central does not store it.

Try:

Follow

New articles from what you follow go into your email digest, once you agree to alert emails.

  • JournalJournal of Nanomedicine & Nanotechnology
  • SubjectNanotechnology
  • BylineArticles whose byline prints “Shien-Uang Jen”