The recently introduced method of twin polymerization is a synthesis route to produce nanoporous hybrid materials, containing organic and inorganic structure domains of 0.5 to 3 nm in a large variety of different compositions. Although first theoretical and experimental investigation has been performed, the open question still remains: How does the structure formation process of twin polymerization, yielding these interweaved organic-inorganic nanoporous hybrid materials, takes place in detail? Understanding the occurring effects and processes of the structure formation opens up the possibility to design (organic and/or inorganic) nanoporous materials with desired properties for industry. E.g. nanoporous materials are of great interest in applications like gas filter systems, catalyst or fuel cells. Here, we present a possibility to derive kinetic reaction parameters as the activation energy barrier or the reaction rate constant by fitting differential scanning calorimetry data via an equation system obtained from reaction kinetics. Recent Publications 1. Hoffmann KH, Prehl J (2018) Modeling the structure formation process of twin polymerization, Reaction Kinetics, Mechanism and Catalysis 123:367-383. 2. Prehl J, Schönfelder T, Friedrich J, Hoffmann KH (2017) Site dependent atom type ReaxFF for the proton-catalyzed twin polymerization. Journal of Physical Chemistry C 121:15984- 15992. 3. Lang J, Prehl J (2017) An embarrassingly parallel algorithm for random walk simulations on random fractal structures. Journal of Computational Science 19:1-10. 4. Prehl J, Boldt F, Hoffmann KH, Essex C (2016) Symmetric fractional diffusion and entopy production. Entropy 18:275. 5. Tchernook I, Prehl J, Friedrich J (2015) Quantum chemical investigation of the counter anion in the acid catalyzed initiation of 2,2â??-spirobi[4H-1,3,2-benzodioxasiline] polymerization. Polymer 60:241-251. 6. Schönfelder T, Friedrich J, Prehl J, Seeger S, Spange S, Hoffmann KH (2014) Reactive force field for electrophilic substitution at an aromatic system in twin polymerization. Chemical Physics 440:119-126.

Subjects

Chemistry

Ask about this article

Answers come only from this article's title, abstract and keywords, each sentence pointing to where it comes from. Your question is sent to OpenAI to write the answer. Scholars Central does not store it.

Try:

Follow

New articles from what you follow go into your email digest, once you agree to alert emails.

  • JournalJournal of Physical Chemistry & Biophysics
  • SubjectChemistry
  • BylineArticles whose byline prints “Janett Prehl”
  • BylineArticles whose byline prints “Karl Heinz Hoffmann”
  • BylineArticles whose byline prints “Peter Salamon”