Conference abstractPublished 5 Oct 2018
Stress determination and manufacturing device of a bow-shaped specimen for testing metal stress corrosion
Shenzhen University, P.R China
Abstract
Select any words in the title or abstract, or press this and choose a sentence.
This paper presents a method to determine the stress of a bow-shaped specimen and its manufacturing device, aiming at studying the stress corrosion of steel wire. The specimen is composed of curved bow frame and steel wire. The arch frame exerts a tensile stress on steel wire, which is one of the necessary prerequisites for the study of stress corrosion of metal wire. Based on the assumption of the geometry of the bow form and knowledge of mechanics, a semi-analytical model for determining the tensile stress of steel wire is established, and the main influence parameters are subsequently extracted. The accuracy and applicability of the semi-analytical model are evaluated by the experimental results. On this basis, a simple device for manufacturing the bow-shaped specimens is developed, which enables the mass production of bow-shaped specimens with target tensile stress level, and which significantly improves the efficiency of statistical tests for stress corrosion of metallic wire.
Ask about this article
Answers come only from this article's title, abstract and keywords, each sentence pointing to where it comes from. Your question is sent to OpenAI to write the answer. Scholars Central does not store it.
Conferences in this field
Upcoming conferences in this field.
Follow
New articles from what you follow go into your email digest, once you agree to alert emails.
- JournalJournal of Civil and Environmental Engineering
- SubjectEngineering
- SubjectEnvironmental & Earth Sciences
- BylineArticles whose byline prints “Dawang Li”
- BylineArticles whose byline prints “Jiazhao Liu”
- BylineArticles whose byline prints “Feng Xing”
- BylineArticles whose byline prints “Shaobang Xing”
- BylineArticles whose byline prints “Yingwu Zhou”