Scholars Central

Research articlePublished 3 May 2019

Metal attack and dissolution of scale by mixtures o f acids

Authors: Shalini Srivastava

Der Pharma Chemica

Volume 7 · Issue 8 · Pages 241–245

Ask about this article

Abstract

Select any words in the title or abstract, or press this and choose a sentence.

Calcareous deposits are formed on boiler surfaces b y continuous use of natural water. Scales formed by natural water cannot be removed easily by using single acid . Mixtures of acids were taken to observe metal att ack by acids and descaling. Experiments were conducted in such a manner that the quantity of one acid was gradually increased and the ratio of two acids was kept constant. When HNO 3 concentration was changed, lower concentration decreased rate of corrosion but higher quantities i ncreased it in HCl + H 2 CrO 4 mixture. Results obtained with different concentration of HCl showed acceleration in rate of corrosion in lower concentration of HNO 3 , H 2 CrO 4 mixture. Even in higher concentration weight loss was appreciable. In H 2 CrO 4 HCl , HNO 3 ( 90+5+5 ) respectively mixture is advantageous i.e. corrosion rate is mini mum 0.064 gm/dm 2 and scale dissolution is maximum (0.14 gm/minute).

Ask about this article

Answers come only from this article's title, abstract and keywords, each sentence pointing to where it comes from. Your question is sent to OpenAI to write the answer. Scholars Central does not store it.

Try:

Follow

New articles from what you follow go into your email digest, once you agree to alert emails.

  • JournalDer Pharma Chemica
  • SubjectPharmaceutical Sciences
  • BylineArticles whose byline prints “Shalini Srivastava”