Abstract

Select any words in the title or abstract, or press this and choose a sentence.

In order to improve the cycling performance of LiMn2O4 based cathode materials, we have synthesized a new composition LiCo0.4Al0.1Mn1.5O4 by sol-gel method. In the path of the material synthesis, citric acid was added to serve as a binding agent and a gelling agent respectively, followed by calcinations at 850°C for 12 h. The synthesized material was well characterized by TG/DTA, XRD, FTIR, EPR, SEM, electrical and electrochemical tests. It was found that LiCo0.4Al0.1Mn1.5O4 powder has an ordered cubic spinel phase (space group Fd3m) and exhibits good rate capability. The electrical and electrochemical characterization was carried out in CR-2032 coin type cell configuration. The material delivers an initial discharge capacity of 48 mAhg-1 between 3.5 and 4.9 V at a C/10 rate and subjected for more than 30 cycles. The electrochemical behavior is well supported with impedance data.

Ask about this article

Answers come only from this article's title, abstract and keywords, each sentence pointing to where it comes from. Your question is sent to OpenAI to write the answer. Scholars Central does not store it.

Try:

More from this journal

The newest in Journal of Advanced Chemical Engineering.

All its articles

Conferences in this field

Upcoming conferences in this field.

Follow

New articles from what you follow go into your email digest, once you agree to alert emails.

  • JournalJournal of Advanced Chemical Engineering
  • SubjectChemistry
  • SubjectEngineering
  • BylineArticles whose byline prints “Nayaka GP”
  • BylineArticles whose byline prints “Pai KV”
  • BylineArticles whose byline prints “Manjanna J”
  • BylineArticles whose byline prints “Anjaneya KC”
  • BylineArticles whose byline prints “Periasamy P”
  • BylineArticles whose byline prints “Tripathi VS”